Influence of the Al /clay ratio on the pillaring process of smectite

Smectite-type clays from the state of Pará, Brazil, were characterized by XRD, 27Al MAS NMR, FTIR and textural analysis by nitrogen adsorpition-desorption isotherms. In the production of pillared clays, the Al13 ion (keggin's ion) was used. This ion was obtained by the reaction of AlC(l3)6H2O/NaOH solutions with OH/Al=2 molar ratio and with Al/clay ratios of 5, 10, 15, 20, 25 meq/g of clay, intercalated at 25 ºC during 3 h and calcined at 450 ºC (adequate temperature for calcination). The results showed that the pillarization process increased the basal spaces of the natural clay from 14.02 to 18.84 Å and the surface area from 44.30 to 198.03 m²/g (Al/g of clay = 25 meq/g of clay, pH=4). Materials prepared with different Al/g clay ratio showed the maximum Al incorporation for Al/g of clay = 25 meq/g of clay. The thermal stability of the natural clay was improved by the pillaring procedure.

pillared clay; Al13; smectite


Associação Brasileira de Cerâmica Av. Prof. Almeida Prado, 532 - IPT - Prédio 36 - 2º Andar - Sala 03 , Cidade Universitária - 05508-901 - São Paulo/SP -Brazil, Tel./Fax: +55 (11) 3768-7101 / +55 (11) 3768-4284 - São Paulo - SP - Brazil
E-mail: ceram.abc@gmail.com