Acessibilidade / Reportar erro

Iron extraction from Brazilian smectite by dithionite-citrate-bicarbonate method

A natural clay from Campina Grande region (Paraíba, Brazil), with 8.57% of Fe2O3, was used to study the most appropriate condition to carry out the iron extraction, without altering the clay structure in a significant way. Samples were treated with the Dithionite-Citrate-Bicarbonate method (DCB) for 30 and 120 minutes (pH=9.1), and also with citric acid (pH=1.8; time=15min), at 75°C. Conductivity measurements, X-ray fluorescence, X-ray diffraction, energy-dispersive spectrometry, electron-diffraction with transmission electron microscopy and textural evaluation by nitrogen adsorption were done. The treatment in a basic medium was more selective for iron removal than in acid condition. The time of 30 minutes, with 1.6 g Na2S2O4/10 g clay, was the best condition for the iron extraction.

brazilian clay; smectite; iron extraction


Sociedade Brasileira de Química Secretaria Executiva, Av. Prof. Lineu Prestes, 748 - bloco 3 - Superior, 05508-000 São Paulo SP - Brazil, C.P. 26.037 - 05599-970, Tel.: +55 11 3032.2299, Fax: +55 11 3814.3602 - São Paulo - SP - Brazil
E-mail: quimicanova@sbq.org.br