Influência do lantânio nas propriedades elétricas do titanato de bário obtido por síntese hidrotérmica

Barium titanate powders were produced by hydrothermal synthesis, at 220ºC, for 20 hours, in stoichiometric composition and doped with lantanum varying from 0.2 to 1.0mol%.The powders were characterized by x-ray diffraction and then pressed at 3,000 kgf to form discs. The discs were sinterized on air at 1250ºC for 5 hours and characterized by x-ray diffraction, scanning electron microscopy and complex impedanciometry

Hydrothermal synthesis; doping; sinterizing