El Zohairy et al.1212.El Zohairy AA, De Gee AJ, Mohsen MM, Feilzer AJ. Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks. Dent Mater. 2003 Nov;19(7):575-83. doi: 10.1016/s0109-5641(02)00107-0. https://doi.org/10.1016/s0109-5641(02)00...
(2003) |
Netherlands |
Feldspathic |
Syntac OptiBond Solo Plus Scotchbond |
Tetric flow Nexus 2 RelyX ARC |
24h |
Bond strength/ Microtensile |
Adhesive |
+ for OptiBond = for Syntac and Scotchbond |
El Zohairy et al.1818.El Zohairy AA, De Gee AJ, Hassan FM, Feilzer AJ. The effect of adhesives with various degrees of hydrophilicity on resin ceramic bond durability. Dent Mater. 2004 Oct;20(8):778-87. doi: 10.1016/j.dental.2003.05.010. https://doi.org/10.1016/j.dental.2003.05...
(2004) |
Netherlands |
Feldspathic |
Syntac OptiBond Solo Plus Visio Bond |
Tetric flow Nexus 2 |
1 day, 7 days and 28 days. |
Bond strength/ Microtensile |
Adhesive |
- ou = |
Peumans et al.1919.Peumans M, Hikita K, De Munck J, Van Landuyt K, Poitevin A, Lambrechts P, et al. Effects of ceramic surface treatments on the bond strength of an adhesive luting agent to CAD-CAM ceramic. J Dent. 2007 Apr;35(4):282-8. doi: 10.1016/j.jdent.2006.09.006. https://doi.org/10.1016/j.jdent.2006.09....
(2007) |
Japan |
Leucite |
Heliobond |
Variolink II |
24h |
Bond strength/ Microtensile |
Adhesive |
= |
Meng et al.2020.Meng X, Yoshida K, Atsuta M. Microshear bond strength of resin bonding systems to machinable ceramic with different surface treatments. J Adhes Dent. 2008 Jun;10(3):189-96.(2008) |
Japan |
Leucite |
Heliobond |
Variolink II |
24h or 10,000 cycles of TC. |
Bond strength/ Microshear |
Mixed |
- |
Passos et al.2121.Passos SP, Valandro LF, Amaral R, Ozcan M, Bottino MA, Kimpara ET. Does adhesive resin application contribute to resin bond durability on etched and silanized feldspathic ceramic? J Adhes Dent. 2008 Dec;10(6):455-60(2008) |
Brazil |
Feldspathic |
Scotchbond |
Variolink II |
Immediate or 12,000 cycles of TC+ 50 days of storage |
Bond strength/ Microtensile |
Mixed |
- |
Lise et al.2222.Lise DP, Perdigão J, Van Ende A, Zidan O, Lopes GC. Microshear bond strength of resin cements to lithium disilicate substrates as a function of surface preparation. Oper Dent. 2015 Sep-Oct;40(5):524-32. doi: 10.2341/14-240-L. https://doi.org/10.2341/14-240-L...
(2015) |
Brazil |
Lithium disilicate |
ExciTE F DSC |
Variolink II Multilink Automix RelyX Unicem 2 |
24h |
Bond strength/ Microshear |
Adhesive |
= |
Elsayed et al.2323.Elsayed A, Younes F, Lehmann F, Kern M. Tensile bond strength of so-called universal primers and universal multimode adhesives to zirconia and lithium disilicate ceramics. J Adhes Dent. 2017;19(3):221-8. doi: 10.3290/j.jad.a38436. https://doi.org/10.3290/j.jad.a38436....
(2017) |
Germany |
Lithium disilicate |
Scotchbond Universal; OptiBond XRT; All Bond Universal; Prime e Bond NT |
Variolink Esthetic DC RelyX Ultimate NX 3 Calibra Esthetic |
3 days, 30 days and 7500 cycles of TC or 150 days 37,500 cycles of TC |
Bond strength/ Tensile |
Cohesive |
= |
Murillo-Gómez et al.1313.Murillo-Gómez F, Rueggeberg FA, De Goes MF. Short- and long-term bond strength between resin cement and glass-ceramic using a silane-containing universal adhesive. Oper Dent. 2017 Sep/Oct;42(5):514-25. doi: 10.2341/16-211-L. https://doi.org/10.2341/16-211-L...
(2017) |
Brazil |
Lithium disilicate |
Single Bond Plus; Scotchbond Universal |
RelyX Ultimate |
24h or 6 months |
Bond strength/ Microshear |
Cohesive |
= |
Ataol and Ergun2424.Ataol AS, Ergun G. Effects of surface treatments on repair bond strength of a new CAD/CAM ZLS glass ceramic and two different types of CAD/CAM ceramics. J Oral Sci. 2018;60(2):201-211. doi: 10.2334/josnusd.17-0109. https://doi.org/10.2334/josnusd.17-0109...
(2018) |
Turkey |
Lithium disilicate Zirconia-reinforced lithium silicate |
Clearfil Universal Bond |
Clearfil Majesty ES-2 |
24h or 5,000 cycles of TC |
Bond strength/ Shear |
Adhesive |
- |
Romanini-Junior et al.1616.Romanini-Junior JC, Kumagai RY, Ortega LF, Rodrigues JA, Cassoni A, Hirata R, et al. Adhesive/silane application effects on bond strength durability to a lithium disilicate ceramic. J Esthet Restor Dent. 2018 Jul;30(4):346-51. doi: 10.1111/jerd.12387. https://doi.org/10.1111/jerd.12387...
(2018) |
Brazil |
Lithium disilicate |
XP Bond; Scotchbond Universal |
SureFil SDR Flow |
24h and 12 months |
Bond strength/ Microshear |
Adhesive |
+ in 24h - or = in 12 months |
Barbon et al.1717.Barbon FJ, Moraes RR, Isolan CP, Spazzin AO, Boscato N. Influence of inorganic filler content of resin luting agents and use of adhesive on the performance of bonded ceramic. J Prosthet Dent. 2019 Dec;122(6):566.e1-566.e11. doi: 10.1016/j.prosdent.2019.09.013. https://doi.org/10.1016/j.prosdent.2019....
(2019) |
Brazil |
Feldspathic |
Adper Single Bond 2 |
RelyX Veneer and 3 experimental resin cements |
Immediate |
Bond strength/ Microtensile |
Mixed |
= or + depending on resin cement. |
Flexural strength/ Biaxial |
Fracture |
= or - depending on resin cement. |
Chen et al.2525.Chen B, Lu Z, Meng H, Chen Y, Yang L, Zhang H, et al. Effectiveness of pre-silanization in improving bond performance of universal adhesives or self-adhesive resin cements to silica-based ceramics: chemical and in vitro evidences. Dent Mater. 2019 Apr;35(4):543-53. doi: 10.1016/j.dental.2019.01.010. https://doi.org/10.1016/j.dental.2019.01...
(2019) |
China |
Lithium disilicate |
Single Bond Plus; All Bond Universal |
RelyX Veneer Clearfil AS Luting RelyX Unicem |
24h or 20,000 cycles of TC and 120 days of storage |
Bond strength/ Shear |
Mixed |
+ |
Murillo-Gómez et al.2626.Murillo-Gómez F, Wanderley RB, De Goes MF. Impact of silane-containing universal adhesive on the biaxial flexural strength of a resin cement/glass-ceramic system. Oper Dent. 2019 Mar/Apr;44(2):200-9. doi: 10.2341/17-356-L. https://doi.org/10.2341/17-356-L...
(2019) |
Brazil |
Lithium disilicate |
Adper Single Bond Plus; Single Bond Universal |
RelyX Ultimate |
24h |
Flexural strength/ Biaxial |
Fracture |
= |
Tribst et al.2727.Tribst JPM, Monteiro JB, Venturini AB, Pereira GKR, Bottino MA, Melo RM, et al. Fatigue failure load of resin-bonded simplified lithium disilicate glass-ceramic restorations: effect of ceramic conditioning methods. J Adhes Dent. 2019;21(4):373-81. doi: 10.3290/j.jad.a43000. https://doi.org/10.3290/j.jad.a43000....
(2019) |
Brazil |
Lithium disilicate |
Single Bond Universal; Multilink N Primer A and B |
Multilink N |
24h up to a maximum of 7 days |
Fatigue failure load/ Staircase test |
Radial crack |
= |
Südbeck et al.2828.Südbeck JM, Jacker-Guhr S, Lührs AK. Do different pretreatment methods influence the microtensile bond strength of composite cements to silicate ceramic? J Adhes Dent. 2021 Jul;23(4):335-345. doi: 10.3290/j.jad.b1650153. https://doi.org/10.3290/j.jad.b1650153....
(2021) |
Germany |
Leucite or Lithium disilicate |
Scotchbond Universal |
Variolink Esthetic DC RelyX Ultimate |
24h or 6 months |
Bond strength/ Microtensile |
Mixed |
- |