Abstract
Spread of fire through facades via leapfrog remains a frequent topic in scientific articles due to its destructive potential, compounded by the growing use of curtain walls in high-rise buildings. Unlike other countries, Brazil does not have a national standard with a specific test methodology to evaluate perimeter fire barrier systems. This study aims to investigates the fire safety of glazed facades with measures prescribed by Brazilian legislation and the behavior of the fire plume during the fire event. The analysis is based on the methodologies described in standards E2307 (ASTM, 2020) and E2874 (ASTM, 2019). It was found that the perimeter seal resisted fire until the adjacent glass broke, at which point the measured temperatures exceeded the permitted limits, resulting in the loss of vertical compartmentation. As a scientific contribution, this article tested for the first time the system described in Brazilian regulations using a standardized test methodology to evaluate its performance, highlighting the importance of a global analysis due to the complexity of variables influencing fire spread in glazed facades.
Keywords
Fire safety; Vertical compartmentation; Perimeter fire barrier; Glazed facade; Leap frog
Resumo
Propagação do fogo pelas fachadas via leap frog continua sendo tema frequente em artigos científicos devido ao seu potencial destrutivo, agravado pelo crescente uso de fachadas cortinas em edifícios altos. Ao contrário de outros países, o Brasil não possui norma nacional com metodologia de teste específica para avaliar barreiras perimetrais contra incêndio. O estudo tem como objetivo investigar a segurança contra incêndio de fachadas envidraçadas com medidas prescritas pela legislação brasileira e o comportamento da pluma de fogo durante o incêndio. A análise é baseada nas metodologias descritas nas normas E2307 (ASTM, 2020) e E2874 (ASTM, 2019). Constatou-se que a selagem perimetral resistiu ao fogo até a quebra do vidro adjacente, momento em que as temperaturas medidas excederam os limites permitidos, resultando na perda da compartimentação vertical. Como contribuição científica, o artigo testou pela primeira vez o sistema descrito nas regulamentações brasileiras através de metodologia normatizada para avaliar seu desempenho, destacando a importância da análise global devido à complexidade de variáveis que influenciam a propagação do fogo em fachadas envidraçadas.
Palavras-chave
Fachada envidraçada; Segurança contra incêndio; Compartimentação vertical; Barreiras perimetrais; Leap frog
Introduction
Fires are frequent disasters in urban centers, with consequences that may include casualties, economic losses, and severe damage to the development of cities and society, especially when they occur in high-rise buildings (Sun et al., 2023a). In recent years, facade-propagated fires have been significantly increasing since 2009 reaching an average of 4.8 yearly events worldwide, which is a concerning trend (Bonner et al., 2020; Sun et al., 2023a). The facade represents one of the most complex and expensive systems in building construction, accounting for up to 25% of the total construction cost, and also serving as a means of fire spread to adjacent floors (Liu; Fischer, 2022; Sun et al., 2023a).
Fire safety requirements are paramount when analyzing the performance of buildings, whether during the design, construction, or operation and maintenance phases (Ono; Venezia; Valentin, 2008). Globally, fire safety is regarded as a science, with specific requirements for building materials and components, along with the development of new technologies and the improvement of legislation and standards (Carlo, 2008). Unfortunately, simulating a real fire scenario in a structure is a highly complex activity that depends on various variables and factors, as each fire has its own unique peculiarities that directly influence the maximum temperature reached, duration and heating rate (Helene; Britez; Carvalho, 2019).
The use of glazed facade systems in buildings has been increasing in major commercial centers and Brazilian capitals. Curtain wall facades systems can be characterized as glass panels with vertical mullions and horizontal transoms, involving heterogeneous materials with specific technical requirements and its proper performance depends on a complex framework marked by interdisciplinarity (Chen; Lu, 2018).
Glazed facades are a technique which has been used by designers to make constructions aesthetically appealing and imposing, as well as for their ability to use different glass compositions in order to reduce energy consumption and increase internal lighting (Wang et al., 2017). This fact can be viewed as a concern for fire safety due to the fragility of this system, which may compromise vertical compartmentation in buildings (Gandhi et al., 2017; Wang et al., 2016).
Facades can be one of the fastest pathways for fire propagation in a building, constituting a significant potential route for the spread of fire to the upper floors. This rapid spread is favored by a convergence of several factors, including abundant oxygen, the verticality of the propagation medium, wind, and other atmospheric conditions, which can greatly intensify the fire’s behavior and complicate firefighting efforts (Forero, 2019). According to Forero (2019), the fire propagation through the facades can occur due to four main causes, whether independently or in combination with two or more factors, which are:
-
leap frog effect, characterized by the rapid propagation of flame through windows;
-
propagation through the gap between the floor slab and the facade;
-
propagation through ventilated cavities, which can amplify the spread of fire; and
-
propagation through combustible cladding.
The leap frog effect refers to the fire’s ability to propagate upward through the building’s facade openings, with intense flames and heat capable of breaking the glass of the windows on the upper floors and spreading the fire to higher levels (Forero, 2012). This phenomenon becomes even more dangerous when fueled by strong winds or when combustible materials are present in the facade system, which further accelerates the fire's spread, making it more difficult to control and extinguish. Understanding this effect is crucial for improving fire safety in high-rise buildings.
This effect has become an even more severe risk when analyzing fire safety in tall buildings (Gunasekaran; Premalatha; Malini, 2010). According to the authors, there are only two ways to prevent this phenomenon from occurring: by supporting the facade system directly on the building’s structure and extending the slab through the facade; and, in situations where the facade is external to the structure, using perimeter fire barriers with fire seals at the junction between the slab and the facade system.
The spread of fire between floors through the facade of the building is the subject of several studies, applying different methods of analysis to study various facade systems, materials, and geometries (Anderson et al., 2017). The building's shape, window geometry, and external conditions are crucial for the occurrence of fire spread over the building's exterior (Patterson, 1993). The impact of the window geometry on the flames exiting through the window was also noted by Rodrigues (2009), who concluded that narrower windows or those with similar height and width dimension result in a greater distance of the heated flames from the facade. In contrast, openings with widths significantly greater than their height project flames close to the exterior facade.
Using computational simulation models, a detailed comparative analysis was conducted on a two-story structure with the same heat source (maximum capacity of 3,500 kW), while varying both window dimensions and ceiling heights to better understand their impact on fire behavior (Schabowicz et al., 2022). Group 1 had windows with a width of 1.20 meters and varying heights, Group 2 had windows with a width of 1.50 meters and varying heights, and Group 3 had windows with a width of 1.20 meters extending to the ceiling. Additionally, the ceiling heights were adjusted to 2.75 meters, 3.25 meters, and 3.75 meters to simulate different scenarios. The results of this study clearly indicated that smaller windows significantly increase the likelihood of the leap frog effect, due to the restricted airflow and the behavior of the flames when in close proximity to the facade. The authors also concluded that with bigger ceiling heights and larger windows, it would influence the way the fire spread along the facade, allowing the fire plume to spread further the facade, avoiding fire propagation through upper floors.
The intersection of the facade system with the building's structure is a critical point in fire safety, especially when using curtain walls, which depend on complex execution, leaves no margin for error, and require specific materials (Forero, 2012). Furthermore, inadequate fire protection seal system, even when installed in the right locations, do not ensure the necessary vertical compartmentation of the perimeter barriers for fire safety (Srivastava; Nakrani; Ghoroi, 2020).
The junctions between the structure and the perimeter barriers are vulnerable points. Since flame spread to adjacent floors can occur, the installed sealing must have the same fire resistance as the structural slab (Sȩdłak et al., 2017). Thus, the fire-stopping seal is appropriately characterized by its essential function, as a barrier against fire spread for fire safety in buildings.
The proper installation of the fire-stopping seal makes a significant difference in the dynamics of a fire. According to a study conducted by Srivastava, Nakrani and Ghoroi (2020), in an environment without the use of a fire-stopping seal, the fire reached two upper floors within thirteen minutes of ignition. On the other hand, with the compartmentation system in place, there was no vertical fire spread during the entire duration of the test.
In a glazed facade, the collapse of glass plates during a fire represents a crucial moment in the dynamics of fire spread. This event creates an oxygen inlet channel into the building and allows the flames to reach the external face of the facade and the upper floors (Wang et al., 2017). The main factors that influence glass breakage are the type of glass, the distance of the fire from the glass, and the fixation method (Wang et al., 2018).
When there is an opening in the facade that provides an oxygen supply, especially after flashover, at which point the fire becomes ruled by the amount of oxygen available in the environment, two distinct flows occur at the window: hot air and flames exit through the upper part of the opening, while oxygen from the external environment enters through the lower part of the window. This continuous exchange of gases further intensifies the fire, as the influx of oxygen sustains the combustion process, allowing the fire to grow and spread more rapidly within the structure (Buchanan, 2001).
Given its importance, there is a large number of scientific publications including mathematical models proposed for estimating the shape and size of the fire plume (Nakrani; Srivastava, 2023; Schabowicz et al., 2022; Sun et al., 2023b), as well as different tests to understand the actual behavior of the fire after being ejected through a facade window, called leap frog effect, ranging from reduced-scale models (Wang et al., 2023) to full-scale (Cancelliere et al., 2020; Li; Wang; Huang, 2022; Nakrani; Srivastava, 2023), and computer simulations (Schabowicz et al., 2022). It is known that the larger the scale of a fire safety test (Gunasekaran; Premalatha; Malini, 2010), the greater its cost and complexity. However, it is the way to approach the real behavior of a facade in a fire situation and to verify the results obtained in computer simulations, smaller-scale tests, and mathematical models.
The vertical compartmentation and the fire propagation could vary considering the internal height of the floor and the position of the perimeter fire barrier, which aspects would influence at the leap frog effect (Forero, 2012; Schabowicz et al., 2022).
Another form of fire propagation that requires careful analysis is through heat flux, which can reach much greater distances than those caused by direct contact with flames and hot gases (Carlsson, 1999). According to the author, this type of heat transfer can significantly contribute to fire spread in adjacent or upper structures or materials. Typical values at which wood ignition can occur are 33.5kW/m² for spontaneous ignition and 12.5kW/m² for ignition in the presence of a source, such as ash or a spark, when preheated (Barnett, 1989). These thresholds demonstrate how dangerous heat flux can be, even without direct flame exposure.
When a building is exposed to heat flux, materials susceptible to ignition include both those on the facade and those inside the rooms with openings to the exposed facade (Barnett, 1989). To prevent ignition due to incident radiation, the author suggests that design limits should be established, considering whether the ignition occurs spontaneously or with the presence of an external source.
The heat flux limit should be set at 12.5 kW/m² in situations where the facade is non-combustible and with combustible materials just inside the widow, due to the usage of ordinary glazing for enclosure, as it would easily break, allowing flying brands to enter and potentially start a fire. In contrast, for fire-resistant glass that does not break or fall during the designed period, a threshold value of 25 kW/m² can be set for spontaneous ignition of materials inside the room (Barnett, 1989). Considering internal materials, Pesic et al. (2017) defined as 10 kW/m² the heat flux threshold for cotton.
Considering that there are different ways that a fire can propagate along the facade (Barnett, 1989; Konecki; Gałaj, 2017), this article will address facades made of incombustible materials, considering the leap frog effect and the fire plume ejected through the window. This effect is one of the most fundamental problems in a building's fire dynamics and can be considered the most severe and frequent due to the direct incidence of flames on the external face of the facade (Oleszkiewicz, 1990).
Regarding building facades, there is an international concern about the performance of facade systems in fire situations. Different countries have adopted various methods to assess the behavior of the systems that make up building facades. However, in Brazil, there is still no specific Brazilian technical standard for testing perimeter barrier systems. Therefore, an American methodology was adopted to enable the analysis proposed by this study.
Therefore, in this work, a full-scale experiment was conducted, simulating two floors with a window on the lower floor, to analyze the fire safety of glazed facades with all the safety measures prescribed by Brazilian legislation which establishes the constructive solution and the behavior of the fire plume throughout the development of the fire.
Methods
The present experimental program aimed to simulate a fire scenario with external fire spread to upper floor of a building facade through a window, as well as to calibrate the equipment proposed by standard E2307 (ASTM, 2020) and E2874 (ASTM, 2019) for testing the fire safety of perimeter fire barrier system prescribed by the technical instruction which establishes the constructive solution at Brazil. The test was conducted at Technological Institute for Performance and Civil Construction (Itt Performance), located at São Leopoldo/Brazil. This section is divided into two subsections: apparatus structure and calibration, which explain the composition of the apparatus, equipment, thermal treatment and the calibration wall and procedure.
Apparatus structure and calibrations
The test apparatus constructed for this research simulates a two-story building with a height of 5.60 meters. The first floor is designated as the test room and the second is the observation room. Both rooms have internal dimensions of 2.50 meters in width, 2.0 meters in depth, and 2.50 meters in height.
The equipment structure comprises four precast reinforced concrete galleries stacked two by two (Figure 1). The concrete used in the galleries has a strength of 20 MPa.
The back closure of the galleries was made with drywall, where, on the first floor, the internal face is composed of 15 millimeter fire-resistant gypsum boards, a 128 kg/m³ density ceramic blanket insulation, and the external face with a standard gypsum board. The upper floor closure was made with a standard gypsum board on both faces.
The test room received thermal insulation with 15 millimeter thick fire-resistant gypsum boards and a 128 kg/m³ density ceramic blanket. The lateral walls, back, and ceiling were covered with a layer of gypsum boards and a layer of ceramic blanket. The floor was covered with two layers of 15 millimeter fire-resistant gypsum boards and a 128 kg/m³ density ceramic blanket, as shown in Figure 2.
The apparatus was equipped with two burners, one inside the test room and another outside, both rectangular in shape.
The external burner was rectangular shaped, with a 1.524 x 1.3 meter long piece of nominal 51 millimeters stainless-pipe, with an upward facing slot having width and length measuring of 13 millimeters by 1.118 millimeters, supplied by liquefied petroleum gas (LPG) through a steel pipe with outside diameter of 25 millimeters and a “T” junction at the back of the window burner to provide uniform gas pressure at the burner slot. The external burner, including the slot, was wrapped with a layer of 25 millimeters thick ceramic fiber insulation, with density of 128 kg/m³. It was placed 76 millimeters from the exterior face of the exterior wall assembly.
The internal burner was rectangular shaped, with its longitudinal axis 2.00 meters long and its transverse axis 1.524 meters wide, made of 51 millimeters outside diameter stainless-steel pipe. It was drilled upward facing nominal diameter 3.2 millimeters holes in the pipe, located in the front “U” shaped portion of the test room burner. The holes started at a nominal location of 1.066 millimeters from the back wall on both sides the burner and across the front pipe. The holes were placed nominally 25 millimeters on center. The burner was positioned 76 millimeter above the floor of the test room and centered. It was equipped with a gas supply line located outside the apparatus, supplied by liquefied petroleum gas (LPG).
Two Blaster’s rotameters were used to control the gas flow in the burners. The first controlled the external burner with a capacity of 1.6 m³/min and the second controlled the internal burner with a capacity of 3.3 m³/min.
Considering this was the first test performed in the apparatus, it was necessary to run a calibration test according to the American standards E2307 (ASTM, 2020) and E2874 (ASTM, 2019) to evaluate the flow rates of the gas burner, the position of the external burner, the prescribed test room temperatures, exterior temperatures and heat fluxes.
The test wall used for calibration measured 3.50 × 6.00 meters. It consisted of two layers of 15 millimeter thick fire-resistant gypsum boards on each face of the wall, metal profiles spaced at 60 centimeters, with a window with dimensions of 1.98 × 0.762 meters positioned 76.2 centimeters from the test room floor, centered.
The inner part of the wall was covered with a 2.5 centimeter thick, 128 kg/m³ density ceramic blanket. It was also used in the joints between the wall and the concrete structure to avoid heat loss through existing gaps at the junction of the elements.
Temperature data were collected using two sets of Type K thermocouples (T) installed inside the test room (Figure 3), on the external side of the test wall and calibration (Figure 4).
(a) General view of the apparatus structure with the thermocouples at the test room; (b) positioning of thermocouples T19 to T23 inside de test room; (c) general positioning of all thermocouples inside de test room
Three Hukseflux’s water-cooled Schmidt-Boelter heat flux sensors were used and positioned in the observation room during the calibration procedure, aligned to the vertical centerline of the calibration wall, 10 centimeters from the inner face of the calibration wall. The first one positioned 5 centimeters from the floor, the second one 30 centimeters and the third one 60 centimeters from the floor.
On the outside, along the central axis of the wall, 15 thermocouples (T1 to T15) were positioned to record temperatures at different heights of this axis. The first one was positioned at the top of the window opening and the others placed 30 centimeters on center.
Two pressure sensors were positioned in the observation room, vertically aligned with each other, placed 40 centimeters from the inner face of the back wall. The first sensor was installed 50 centimeters from the ceiling, and the second was positioned 76 centimeters from de floor.
The calibration procedure followed E2307 (ASTM, 2020) and E2874 (ASTM, 2019), considering the gas flow rate and burner’s ignition order.
The results demonstrated that the temperatures measured in the apparatus test room met the temperatures established by standards E2307 (ASTM, 2020) and E2874 (ASTM, 2019) throughout the calibration period. This was the only parameter with temperatures to be followed after the first thirty minutes of calibration.
The external temperatures measured met the temperatures established by the standard E2307 (ASTM, 2020) and E2874 (ASTM, 2019) considering the proposed calibration time, which was for one hour.
Glazed facade system
After calibrating the apparatus, a glazed facade, measuring 3.50 × 6.25 meters, with a window positioned 76.2 centimeters from the test room floor, centered, with dimensions of 1.98 × 0.762 meters was installed. Silver 32 OG float 6.0 mm laminated glass, 0.38 polyvinyl butyral (PVB), 4.0 mm float glass, Ecostick aluminum profiles, and Sika brand SG-500 CN two-component structural silicone were used. Figure 5 shows the glazed facade used for the test and the location of the fourteen thermocouples installed along the facade to measure the external temperature. It can be noted that thermocouples numbered 1 to 8 are located on the central glass panel immediately above the window, between two horizontal aluminum profiles.
For the sealing system, a 64 kg/m² density rock wool board with a 100-millimeter thickness was used (Figure 6a), with fibers vertically positioned, a compression rate of approximately 66%, 15 centimeters joint width between the structure and the internal face of the specimen and 1 meter wide for each void. Hilti brand CFS-SP WB red elastomeric paint was then manually applied with a paint thickness of approximately 6.0 mm (Figure 6b).
(a) Rock wool to be installed in the void between the structure and the facade; (b) perimeter seal with rock wool and elastomeric painting
Instrumentation in the sealing was done by placing 22 Type K thermocouples (T23 to T44), distributed as illustrated in Figures 7 to 9.
In the observation room, a vertical drywall system barrier was installed with two layers of 15 millimeter thick fire-resistant gypsum on each face of the wall and studs spaced every 0.60 meter, as illustrated in Figure 10. The total height of this barrier, considering the thickness of the slab, was 1.20 meter.
One Hukseflux’s water-cooled Schmidt-Boelter heat flux sensor was used, positioned at the top of the vertical drywall system barrier, next to the curtain wall facade and inside de observation room, during the test, as illustrated in Figure 10.
Inside the test room, the instrumentation was the same of the calibration procedure, as described at 2.1 Apparatus Structure and Calibrations.
Results and discussion
Internal temperatures
According to E2307 (ASTM, 2020), only the average of the temperatures from thermocouples T19 to T23 is used for controlling internal temperature. The results are shown in Figure 11 along with the standard temperature curve established by standards E2307 (ASTM, 2020) and E2874 (ASTM, 2019) measured by thermocouples T19 to T23. It is noticeable that the temperatures were approximate in meeting the standard curve during the first five minutes of the test, which did not persist due to the low thermal insulation capacity of the glass used. The difference between the measured temperature and the standard curve prescribed is because it must meet during the calibration procedure, then all the equipment would be calibrated. Since calibration wall is made of fire resistance gypsum board and the curtain wall facade test specimen was made of non-fire rated glass, it will result in a different temperature inside the test room when compared to the standard curve.
According to E2307 (ASTM, 2020), during the first five minutes, only the internal burner was activated (Figure 13), and, from the fifth minute onward, the external burner was activated, which also caused the internal temperature to rise. However, this led to the glass breaking and, consequently, internal heat being lost to the environment, making it difficult to increase the temperature in the test room. The decline in temperature after seventy-five minutes of testing was due to the equipment being switched off at the end of the test.
External temperatures
The thermocouples recorded temperatures along the facade which can be grouped into two types based on behavior influenced by the respective heights of the measurement points and test times, which are associated with events that compromised the integrity of the system. These 2 types can be seen in the graph in Figure 12, with thermocouples T1 to T8 distributed up to the limit of the first glass panel and the others, from thermocouple T9 on, located on the glass panel immediately above. Thermocouple T8 is positioned at a height equivalent to the upper limit of the vertical barrier system. The evolution of the temperatures at each thermocouple attachment point and an indication of the main events that occurred during the test were also recorded and are shown in Table 1, with a description of the events and the respective damage to the system. It is worth noting that the ambient temperature at the start of the test was 25 °C.
The points closest to the window (thermocouples T1 to T4) recorded the highest temperatures in the initial minutes of the test. However, their fixation within the system was compromised after the external burner was lit. At that moment, there was a rapid temperature rise, reaching 187 °C at thermocouple T2.
The collapse of the central glass, located immediately above the window, occurred between 5 and 6 minutes from the start of the test when the external burner was activated (Figure 13b). At that moment, thermocouples T1 to T7 recorded temperatures between 54.34 °C and 70.52 °C, respectively. This event was decisive for the loss of system integrity and for the increased flame, which began to reach the external face of the test chamber.
Main events of the first 10 minutes of the test: (a) beginning of the test; (b) partial glass breakage at 6 minutes of test; (c) flamed particles falling from de specimen at 10 minutes of test
Following the lighting of the external burner, between 10 and 15 minutes of the test, there is a plateau in the temperatures recorded on the facade (Figure 12), caused by the exit of hot air through the opening of the broken glass. The temperatures recorded in this event varied between 100.24 °C and 167.98 °C at the points of thermocouples T1 to T7, while at the higher points, with thermocouples 8 to 14, the temperatures were between 85.83 °C and 31.96 °C. At this moment, thermocouple T4 detached and the release of inflamed particles was observed (Figure 13c). These particles are products of the burning and melting of the PVB of the laminated glasses, as the glass break exposed the polymer to direct contact with the flames. Furthermore, it was found that the glass panels not only broke due to high temperatures but also moved downward as the melted PVB accelerated the detachment process.
Approximately 15 minutes into the test, a gradual rise in temperatures is observed in all remaining thermocouples. The side glass near the seal broke at 19 minutes, exposing the rock wool to contact the flames (Figure 14a and Figure 14b). At this point, thermocouples T5 to T7 recorded temperatures between 209.34 °C and 131.79 °C, while the other thermocouples recorded 118.95 °C and 102.34 °C. It should be noted that the thermocouples were fixed in the center of the facade and that the temperatures on the side windows were probably lower.
Main events of the last 20 minutes of the test: (a) glass breakage at 19 minutes; (b) increasing of glass breakage at 20 minutes; (c) aluminum breakdown at 28 minutes; (d) complete glass breakage at 41 minutes of test
At 28 minutes, the horizontal aluminum mount positioned just above the external burner ruptured (Figure 14c). At this moment, the closest thermocouple still fixed to the system, T5, recorded a temperature of 238.18 °C. Between 41 and 43 minutes of the test, the total breaking of the central glass occurs (Figure 14d), the temperature recorded at the sealing reaches 181 °C, and at the point of thermocouple 8, 222.18 °C.
At 51 minutes, the thermocouples T7 and T8 fell. At the highest points of fixation of the thermocouples, the temperature over time had a more homogeneous behavior among the points, with similar graphic profiles and an increase in temperature recording at the lower points. Figures 10 and 11 show the images of the evolution of the flames during the test.
The general aspect of the facade after the burners were turned off is shown in Figure 15. Most of the structure remained intact, with the most significant damage observed at locations of direct flame contact. The three glass panels in contact with the sealing were broken, their respective vertical aluminum mounts were deformed (Figure 15a and Figure 15b), and the top horizontal mount of the window was ruptured (Figure 15c).
Facade after the test: (a) general view; (b) glass breakage above the perimeter seal; (c) aluminum mullion melted and glass brakeage below the perimeter seal
Sealing temperatures
According to E2307 (ASTM, 2020), the fire resistance time of the sealing system is defined as the moment when either the temperature exceeds the limit of 206 °C (181 °C above the initial temperature) or flames penetrate the upper floor through or around the sealing.
The evolution of the temperatures on the upper face of the sealing can be analyzed through the graphs in Figure 16. The temperatures measured in the central axis of the sealing and inside the two main mullions are shown in Figure 16b, revealing a comparatively more pronounced and less homogeneous temperature rise compared to the previous graph. The temperatures inside the mullions differed from the others, mainly in their graphic profile. The highest temperature of 262.85 °C was recorded at T44 and a decrease at T43, both at 40 minutes of the test. This moment marked the break of one of the glasses and the failure of the airtightness of the system. Based on data from Figure 16 and Figure 17, it was observed that temperatures rose more rapidly the closer they were measured to the facade glass, as well as toward the left vertical mullion, where the highest recorded temperature was observed.
Temperatures in fire-resistant sealing: (a)T23, T24, T29, T30, T37 and T38; (b) T25, T26, T31, T32, T33, T39, T40, T43 and T44
In Figure 16c, the evolution of the temperatures near the facade glass can be seen, with points T34, T35, and T36 located in the central module aligned with the external burner. At 19 minutes into the test, when the glass in contact with the sealing broke, two behaviors were observed: a more rapid increase in temperature at T34, T35, and T36, and a slower increase at the other points. The differences at the points near the glass varied from 74.40 °C to 152.61 °C at points T42 and T35, respectively.
Considering the results presented regarding the temperatures measured on the surface of the perimeter sealing, thermocouples T36 and T44 reached 215.90 °C and 262.85 °C, respectively, exceeding the maximum allowable temperature of 206 °C, according to E2307 (ASTM, 2020) and E2874 (ASTM, 2019).
In addition to the temperatures observed, it was noted that the flames passed through the space created by the breaking of the glass next to the sealing, as well as through the sealing installed between the fixing system of the left central mullion, where the highest temperatures were recorded.
The installed vertical barrier ensured that the flames passing through the perimeter sealing did not enter the observation room. The temperatures measured at the top and center of the vertical barrier did not exceed 56 °C (thermocouples T45 and T46). However, the focus of the highest temperatures in the perimeter sealing was not centralized, which could have resulted in higher temperatures than those measured.
Based on the results, it can be concluded that the interfaces between the sealing and the vertical mullions are critical points for damage due to temperature elevation. As such, they require a more careful installation, including the cutting of the material at these points.
Behavior of the fire plume
Through the thermal camera installed on the side of the test, it was possible to observe the behavior of the flame along the facade, the occurrence of the leap frog effect during the test, and the different conformations of the fire tongue due to the glass breakage. During the first five minutes, the most critical moment occurred during the operation of the internal burner, generating a region of hot air exiting through the window, as illustrated in Figure 18a.
After the ignition of the external burner, there was direct flame contact on the vertical axis of the facade, with the warmer air forming a layer parallel to the sample (Figures 18b and 18c).
After the glass sections above the window broke, the hotter air exhibited a less homogeneous conformation (Figure 19). As a result of the rise in temperature caused by the external burner, heat transfer by convection was accelerated, being faster in the layers of air near the highest points, as they have lower temperatures.
The area heated by the flames and hot air doubled in front of the sample after the glass breakage. At 37 minutes into the test, the hottest layer returned to its initial conformation, forming a parallel layer along the facade, following the shape of the flames in the leapfrogging effect.
As the test progressed and with the progression of glass breakage in the sample, there was an increase in the area and height available for the exit of hot air and the entry of cooler air, leading to vertical movement of the neutral line. The behavior of the fire from the external burner was directly affected. It was carried by the flow of cooler air into the test room and then exited along with the hot airflow, as illustrated in Figure 20.
The described behavior is further supported by the internal pressure measurements taken during the test. Unlike what was observed during calibration, the upper part of the test room showed positive pressure (indicating the entry of cooler air), causing the behavior illustrated in Figure 20.
Heat flux at the observation room
During the test, the heat flux steadily grew for a duration of forty-two minutes, ultimately reaching its maximum value of 14.73 kW/m². From then on, the heat flux remained constant until the end of the test, with an average value recorded of 12.10 kW/m².
The maintenance of the heat flux after reaching the maximum value was due to the reduction in glass breakage in the facade, which effectively kept the heat entry through the existing opening constant. Additionally, the fire behavior during this period remained largely unchanged.
Furthermore, it is important to note that the incident heat flux may have been higher than recorded due to the decentralization of the point where the highest temperatures were measured about the heat flux meter positioned at the center of the vertical partition.
Conclusions
This article presented the results of a full-scale experiment that investigated the behavior of a fire initiated on a glazed facade. Data were collected on the internal, external, and upper surface temperatures of the sealing system. In addition, the behavior of the fire plume and the development of the leap frog effect was analyzed.
The decisive event in the evolution of the temperatures inside the test room was the breaking of the lower part of the central glass in the facade. This occurred 5 minutes into the test, with the activation of the external burner, resulting in temperatures on the glass surface reaching 70.52 °C.
The test results demonstrate that the system under study, with perimeter sealing and the fire barrier, maintained vertical compartmentation until the glass broke at the height equivalent to the perimeter sealing, which happened at 40 minutes of the test and then temperatures measured at the perimeter seal exceeded the standard limit, which was 206 °C. The perimeter sealing system was designed to withstand 2 hours of testing, as this is the usual fire resistance time for buildings over 30 meters in height, according to the technical instructions of the fire department. However, it lost its vertical compartmentation capacity after 40 minutes of testing due to the fragility of the system as a whole in the facade and the installation method of the protection system, rather than specifically due to the materials used in the perimeter sealing system. The system would need to maintain the same design resistance time as the rest of the building (Sȩdłak et al., 2017).
The 1.20-meter vertical barrier is aimed to prevent direct fire entry to the upper floor due to the leap frog effect. After the glass breakage, the system was composed of fire-resistant perimeter sealing and the vertical barrier was incapable of ensuring compartmentation between floors due to the presence of fire above the perimeter seal and the heat flux measured at the top of the vertical barrier.
The heat flux emerged in the present study as a fundamental parameter to be considered for the analysis of vertical compartmentation in glass curtain wall facades. This instance, could have potentially led to the ignition of cladding materials, such as preheated cotton and wood, which are commonly used materials for internal finishing (Barnett, 1989; Pesic et al., 2017). This highlights the critical role that heat flux plays in determining fire risk, as well as the need for more precise fire safety strategies when using curtain wall facade systems, particularly in high-rise buildings.
Furthermore, the change in the geometry of the opening in the glazed facade, which resulted in an increased ventilation area during the test, can directly impact the fire’s behavior and propagation along the external face of the sample. After the glass broke, the fire began to move away from the facade upon exiting through the opening, reducing temperatures on the external face and in the perimeter sealing. This behavior is supported by the results presented by the authors Forero (2012) and Schabowicz et al. (2022), who demonstrated the impact of the internal floor height and the positioning of the perimeter fire barrier on the leap frog effect behavior.
This study highlights the importance of having a global view of external fire spread in facades to fully understand the real performance of a glazed facade system when exposed to fire. Variations in flame and heat behavior, due to the complex interaction of different constituent elements of facades and the overall structure of the building when subjected to the high temperatures of a fire, need to be thoroughly considered. Understanding these interactions is essential for developing more effective fire safety measures and improving the resilience of buildings against fire incidents.
As a suggestion, to find a solution based on the system prescribed by technical instructions, it is recommended to conduct tests considering edge beams to modify the distribution of the 1.20 meter vertical barrier, addressing the impact identified at the leap frog effect (Forero, 2012; Schabowicz et al., 2022), or considering the shadow box, usually used to hide the perimeter seal from an outside view.
For further studies, computational modeling can serve as a basis for specifying systems to be tested, as well as for analyzing more complex scenarios, such as a building with more floors or different proportions.
References
- AMERICAN SOCIETY FOR TESTING AND MATERIAL. E2307: standard test method for determining fire resistance of perimeter fire barriers using intermediate-scale, multi-story test apparatus. West Conshohocken, 2020.
- AMERICAN SOCIETY FOR TESTING AND MATERIAL. E2874: standard test method for determining the fire-test response characteristics of a building spandrel-panel assembly due to external spread of Fire. West Conshohocken, 2019.
- ANDERSON, J. et al. Fire dynamics in façade fire tests: Measurement, modeling and repeatability. Applications of Structural Fire Engineering, n. June, 2017.
- BARNETT, C. Fire separation between external walls of buildings. Fire Safety Science, v. 2, p. 841–850, 1989.
- BONNER, M. et al. KRESNIK: A top-down, statistical approach to understand the fire performance of building facades using standard test data. Building and Environment, v. 169, n. August 2019, p. 106540, 2020.
- BUCHANAN, A. Fire engineering design guide Christchurch: University of Canterburry, 2001.
- CANCELLIERE, P. et al. A new test method to determine the fire behavior of façades with etic system. Fire and Materials, n. November 2019, p. 1–14, 2020.
- CARLO, U. del. A segurança contra incêndio no mundo In: A SEGURANÇA contra incêndio no Brasil. São Paulo: Projeto Editora, 2008.
- CARLSSON, E. External fire spread to adjoining buildings: a review of fire safety design guidance and related research. Lund, 1999. 125 f. Bachelor - Science In Fire Protection Engineering, Department of Fire Safety Engineering, Lund University, Lund, 1999.
- CHEN, K.; LU, W. Design for manufacture and assembly oriented design approach to a curtain wall system: A case study of a commercial building in Wuhan, China. Sustainability, v. 10, n. 7, 2018.
- FORERO, M. del P. G. Evaluación del comportamiento del fuego y protección contra incendios en diversas tipologías de fachadas Barcelona, 2012. 409 f. Thesis (Doctorate) – Curso de Arquitectura, Department of Architectural Constructions, Polytechnic University of Catalonia, Barcelona, 2012.
- FORERO, M. del P. G. Propagación del fuego por fachada. In: ESTUDIO sobre la problemática generada por la propagación de incendios en fachadas de edificios. Barcelona, 2019.
- GANDHI, P. et al. Performance of glass-ACP façade system in a full-scale real fire test in a G+2 structure. Procedia Engineering, v. 210, p. 512–519, 2017.
- GUNASEKARAN, U.; PREMALATHA, E.; MALINI, T. P. A. Facades of tall buildings: state of the art. Modern Applied Science, v. 4, n. 12, p. 116–125, 2010.
- HELENE, P.; BRITEZ, C.; CARVALHO, M. Ações e efeitos deletérios do fogo em estruturas de concreto. Uma breve revisão. Revista ALCONPAT, v. 10, n. 1, p. 1–21, 2019.
- KONECKI, M.; GAŁAJ, J. Flame transfer through the external walls insulation of the building during a fire. Procedia Engineering, v. 172, p. 529–535, 2017.
- LI, Y.; WANG, Z.; HUANG, X. An exploration of equivalent scenarios for building facade fire standard tests. Journal of Building Engineering, v. 52, p. 104399, 2022.
- LIU, J.; FISCHER, E. C. Review of large-scale CLT compartment fire tests. Construction and Building Materials, v. 318, n. December 2021, p. 126099, 2022.
- NAKRANI, D.; SRIVASTAVA, G. Full-scale fire performance of combustible and non-combustible curtain wall systems with firestops. Fire Technology, v. 59, n. 1, p. 153–190, 2023.
- OLESZKIEWICZ, I. Fire exposure to exterior walls and flame spread on combustible cladding. Fire Technology, v. 26, n. 4, p. 357–375, 1990.
- ONO, R.; VENEZIA, A. P. P. G.; VALENTIN, M. V. Arquitetura e urbanismo. In: A SEGURANÇA contra incêndio no Brasil. São Paulo: Projeto Editora, 2008.
- PATTERSON, J. Simplified design for building fire safety Iowa State University: John Wiley & Sons, 1993.
- PESIC, D. J. et al. Simulation of fire spread between residential buildings regarding safe separation distance. Tehnicki Vjesnik, v. 24, n. 4, p. 1137–1145, 2017.
- RODRIGUES, E. E. C. Análise da eficiência dos sistemas de compartimentação vertical externa por afastamento entre janelas e por projeções horizontais segundo as exigências normativas brasileiras Porto Alegre, 2009. 178 f. Thesis (Master) – Graduate Program in Civil Engineering, Federal University of Rio Grande do Sul, Porto Alegre, 2009.
- SCHABOWICZ, K. et al. Numerical analysis of storey-to-storey fire spreading. Archives of Civil Engineering, p. 91-109, jan. 2022.
- SȨDŁAK, B. et al. Fire-stop wraps and collars with intumescent materials-performance comparison. Procedia Engineering, v. 172, p. 961–968, 2017.
- SRIVASTAVA, G.; NAKRANI, D.; GHOROI, C. Performance of combustible facade systems with glass, acp and firestops in full-scale, real fire experiments. Fire Technology, v. 56, n. 4, p. 1575–1598, 2020.
- SUN, X. et al. Fundamentals of window-ejected fire plumes from under-ventilated compartment fires: Recent progresses and perspectives. Progress in Energy and Combustion Science, v. 94, n. July 2021, p. 101039, 2023a.
- SUN, X. et al. Transverse and lateral temperature profiles of the window-ejected thermal plume along the facade. Journal of Building Engineering, v. 76, n. July, p. 107303, 2023b.
- WANG, J. et al. Experimental study on upward flame spread over XPS under the influence of facade openings. Journal of Building Engineering, v. 78, p. 107630, 2023.
- WANG, Y. et al. Influence of fire location on the thermal performance of glass façades. Applied Thermal Engineering, v. 106, p. 438–442, 2016.
- WANG, Y. et al. Investigation of thermal breakage and heat transfer in single, insulated and laminated glazing under fire conditions. Applied Thermal Engineering, v. 125, p. 662–672, 2017.
- WANG, Y. et al. Sensitivity analysis of influencing factors on glass façade breakage in fire. Fire Safety Journal, v. 98, n. January, p. 38–47, 2018.